  • This is a motorcycle front viser / headlight surround.
    Wanted to share with you how my homemade formula comes out.

Komentáře • 56

  • @WasimAkram-ck2wb
    @WasimAkram-ck2wb Před 2 lety +1

    Well never knew it was such a task for chrome. I thought we get to buy chrome color and paint it. No wonder its expensive! Great work mate

    • @EssexSilvering
      @EssexSilvering  Před 2 lety

      It's actually silvering (silver plating) just looks like chrome ;-)

  • @craig6299
    @craig6299 Před 3 lety +1

    Very interested in actual formula, I'll be doing my bike

  • @raycoulson4050
    @raycoulson4050 Před 3 lety +3

    Hey Dave, very impressive. I'm hoping to try doing it here in Australia. Could you please give me a list of chemicals and ratios Thanks Ray

    • @EssexSilvering
      @EssexSilvering  Před 3 lety +1

      Main chemicals = Silver Nitrate, Ammonia, Sodium Hydroxide, Hydrochloric Acid, Stannous Chloride ............. And LOADS of water! ;-) .. Ratios no good to anyone as different country's will offer different percentages of chemicals.

    • @kacafilmsemarang9124
      @kacafilmsemarang9124 Před 3 lety

      @@EssexSilvering You awesome with your DIY, what about the order of chemical administration?

    • @rstezza
      @rstezza Před 3 lety

      @@EssexSilvering how about percentages in the U.K.??

    • @EssexSilvering
      @EssexSilvering  Před 3 lety +2

      @@kacafilmsemarang9124 Only order of chemical is the 2 combined that spray together - Silver Nitrate and Sodium Hydroxide + Ammonia.

    • @EssexSilvering
      @EssexSilvering  Před 3 lety

      @@rstezza All my chemicals are from the UK as I live here ;-)

  • @customart5150
    @customart5150 Před 3 lety +1

    Very cool

  • @kingbricolage
    @kingbricolage Před 2 lety +1

    The best explanation of the process I have seen. So bottle A for the duel head sprayer is a combination of Silver nitrate and sodium hydroxide + di water and B is Ammonia + Di water. I haven’t seen people rinse between silvering before either. Your wetting agent and silver sealer home made so what are they made from? I’m an artist in OZ giving this a go on my sculptures. Thanks for your videos Dave :)

    • @EssexSilvering
      @EssexSilvering  Před 2 lety +2

      Bottle A ... Is Silver Nitrate + Sodium Hydroxide (Or Potassium Hydroxide) + Ammonia + DI Water .... Bottle B is actually Sugar (Dextrose) + Ammonia + DI Water ... Wetting agent is a homemade formula that simply consists of a Surfactant with DI Water that is generally used on plants for gardening ... Hope this helps ;-)

    • @kingbricolage
      @kingbricolage Před 2 lety

      @@EssexSilvering thanks Dave I appreciate your help.

  • @ihsanaldulaimy8962
    @ihsanaldulaimy8962 Před 2 lety

    Can i know thr best chemical contents of hydrochrom formula to make it whitter cuz my formula makes it yellowish

  • @opviper895
    @opviper895 Před 7 měsíci

    Sir can you tell me the ingredients of the bottle S (Silver sealer, Anti_oxidant)

  • @ryandavis2025
    @ryandavis2025 Před rokem

    Mate this is awsome. I have been looking to make the formula for this. Any chance of getting the mix ratios you used?

  • @scotteverett7834
    @scotteverett7834 Před 3 lety

    @Dave24v Soooo...any chance of a list and ratios of the chemicals you used?

    • @ayeshasays7398
      @ayeshasays7398 Před 3 lety +1

      Sure

    • @craig6299
      @craig6299 Před 3 lety

      What are the ratios?

    • @EssexSilvering
      @EssexSilvering  Před 2 lety

      Ratio's depend on the strength of the chemicals / acids you have ... So unless you have the same strength as mine that's the only way I could help you ;-)

    • @ankitadeshara8679
      @ankitadeshara8679 Před 3 dny

      ​@@EssexSilvering
      Ok sir, please explain which ratio r u using? With this indication i will prepare ratio with trial and error

  • @aydin3126
    @aydin3126 Před rokem

    Hello, what chemicals do you use for adhesion?

    • @EssexSilvering
      @EssexSilvering  Před rokem +1

      Adhesion is the activator, info is in my other video

  • @MuhammadRidwan-bv5ow
    @MuhammadRidwan-bv5ow Před 3 lety

    Hi bro, what d name first chemical or aktivator before silvering chemical? Please for answer n tq

    • @EssexSilvering
      @EssexSilvering  Před 3 lety

      Activator is Stannous Chloride + Hydrochloric Acid + DI Water.

    • @MuhammadRidwan-bv5ow
      @MuhammadRidwan-bv5ow Před 3 lety

      @@EssexSilvering after mixed must be waiting 24h ? Tq u so much for u sharing brother 👍

    • @EssexSilvering
      @EssexSilvering  Před 3 lety +1

      @@MuhammadRidwan-bv5ow No waiting time , ... You can use onced mixed, ... After mixing will last for about 2 weeks.

    • @MuhammadRidwan-bv5ow
      @MuhammadRidwan-bv5ow Před 3 lety

      How much ratio between 2 chemical to mixing Di Water?

  • @tejasdarekar3250
    @tejasdarekar3250 Před 2 lety

    How to make chemical formula

  • @manojbatham2946
    @manojbatham2946 Před 2 lety

    Sir, what is antioxidant. PLZ. Clarify. 🙏🙏🙏

    • @EssexSilvering
      @EssexSilvering  Před 2 lety

      It's a chemical that creates a water beeding so it's easy to dry and blow the water off.

    • @manojbatham2946
      @manojbatham2946 Před 2 lety +1

      @@EssexSilvering what chemical sir? Please tell that chemical name.

    • @manojbatham2946
      @manojbatham2946 Před 2 lety

      What chemical sir? Please tell that chemical name.

    • @EssexSilvering
      @EssexSilvering  Před 2 lety +1

      @@manojbatham2946 Shampoo, Sulphuric Acid mixed with DI Water. .... Another way is to melt bar of soap and add Sulphuric Acid with DI Water.

  • @venkataramana7108
    @venkataramana7108 Před 2 lety

    After finished do you protect the finish with clear coat

    • @EssexSilvering
      @EssexSilvering  Před 2 lety +1

      Yes, ... I use 2k clear coat with a voilet tint to protect the silver from the UV light (sun)

  • @brokenring1209
    @brokenring1209 Před 2 lety

    It turns to yellow when I spray top coat

    • @EssexSilvering
      @EssexSilvering  Před 2 lety +1

      You have to add some Voilet tint with the clear coat. If you have clear coated and it's looking yellow, don't panic, just give it a second coat with a voilet tint and it will turn shiney silver chrome.

    • @brokenring1209
      @brokenring1209 Před 2 lety +1

      @@EssexSilvering
      Thanks for the information
      I hope epoxy dyes will work

  • @paulsonaivy
    @paulsonaivy Před 2 lety

    the water you are using is not di water, check water ,you should be getting a better finish

    • @EssexSilvering
      @EssexSilvering  Před 2 lety

      It is DI water .. I make it myself and the reading of the water is 0.001 ;-) ... The lighting is not very good in my garage .. This is a different lighting on a wheel I did - czcams.com/video/rJ8W_gC3zwU/video.html

  • @karlbigmore7949
    @karlbigmore7949 Před 3 lety

    Is it expensive

    • @EssexSilvering
      @EssexSilvering  Před 3 lety

      Only expensive chemical is the silver nitrate crystals

    • @karlbigmore7949
      @karlbigmore7949 Před 3 lety

      @@EssexSilvering apc do for 25 I think on ebay

  • @nihalansari9540
    @nihalansari9540 Před rokem

    Sir, can I get your contact please
    I want your Help

  • @lumimobb
    @lumimobb Před 10 měsíci

    Has to be done on 2k clear surface correct?

    • @EssexSilvering
      @EssexSilvering  Před 10 měsíci

      No, ... Silver will have no adhesion on a clear 2K Lacquer, it has to be a 2K basecoat