  • On todays episode of T.C.'s Customs we go over how to do an entropic or flame anodized finish on a set of titanium scales. With a beautiful finish and an outcome that anyone would love to have in their pocket, it's not as hard as you might think...
    Para 3
    www.smkw.com/s...
    All Spyderco
    www.smkw.com/s...
    Titanium Scales
    www.smkw.com/s...
    Custom Shop
    www.smkw.com/s...
    Jantz Ferric Chloride Acid
    www.smkw.com/j...
    See all of our gear here: 👉 www.smkw.com/s...
    Follow our other platforms for more deals!
    Social Media Links:
    CZcams:👉 / smkwcom
    Instagram:👉 / smokymountainknifeworks
    Facebook:👉 / smokymountainknifeworks
    Gettr:👉 gettr.com/user...
    Twitter: 👉 / smkwcom
    TikTok:👉 www.tiktok.com...

Komentáře • 120

  • @jeremynedrow7003
    @jeremynedrow7003 Před rokem +4

    I always wanted to learn how to do this finish thanks TC.

    • @SMKWcom
      @SMKWcom  Před rokem

      Thanks for watching Jeremy!

  • @billpritchett39
    @billpritchett39 Před rokem +2

    Those scales came out beautiful.

    • @SMKWcom
      @SMKWcom  Před rokem +1

      They are very eye-catching and TC has been EDCing it since 👍

  • @shadowdancer8352
    @shadowdancer8352 Před rokem +2

    great video always fun

    • @SMKWcom
      @SMKWcom  Před rokem +1

      Thanks for watching SD!

  • @mikereese15
    @mikereese15 Před rokem +1

    Wow. Awesome end product there TC. Made it look easy

    • @SMKWcom
      @SMKWcom  Před rokem

      Thanks for watching Mike R!

  • @slayingrn
    @slayingrn Před rokem +1

    Awesome video! A real service to the community!

  • @Its_a_knifestyle
    @Its_a_knifestyle Před rokem +1

    My favorite ano finish by far!!

  • @Damen0530
    @Damen0530 Před rokem +2

    Looks awesome 👍👍👍

    • @SMKWcom
      @SMKWcom  Před rokem

      TC did awesome on this one!

  • @garylyman4922
    @garylyman4922 Před rokem +1

    Looks amazing TC.

  • @willb7713
    @willb7713 Před rokem +1

    That looks great TC! I'm getting ready to electro anodize some stuff for the first time.

    • @SMKWcom
      @SMKWcom  Před rokem

      Good luck and hope they turn out awesome!

  • @kjgas6945
    @kjgas6945 Před rokem +1

    Thank you TC

  • @ghostmaloneedc4254
    @ghostmaloneedc4254 Před rokem +2

    So ironic y’all posted this today TC, because I literally just did the same finish on my ASK titanium liners and hardware, and was putting in an order for the TI para3 scales on Friday for the same purpose! Awesome finish

    • @SMKWcom
      @SMKWcom  Před rokem

      Thanks GM!

    • @superrad1659
      @superrad1659 Před rokem +1

      How you liking the ASK?

    • @ghostmaloneedc4254
      @ghostmaloneedc4254 Před rokem

      @@superrad1659 been in my pocket every day since November of last year, so almost a whole year of carrying it, I couldn’t be more pleased. Absolutely fantastic tool. Probably my favorite piece of EDC/knife I own.

    • @ghostmaloneedc4254
      @ghostmaloneedc4254 Před rokem

      @@superrad1659 you can check out some of my reviews and vids I’ve done on the ASK. It’s always with me!

    • @superrad1659
      @superrad1659 Před rokem

      @@ghostmaloneedc4254 bold statement lol thats awesome tho! I havent seen too many reviews on it, mainly just Greg's pre-production and customizing vids. Theres a lot I like about it, just been a lil hesitant given its price. I should prob just shut up and get one in my pocket tho lol.

  • @BluetoothBlades
    @BluetoothBlades Před rokem +1

    Beautiful.

  • @richardcampbell5762
    @richardcampbell5762 Před rokem +1

    I'm diggin it!! I'll be doing it to a few for sure!! Thanks for sharing brother. From New Mexico, Cheers!! 🍻🍻👍🇺🇸🤙🇺🇸✌️

  • @DailyDrivenBikes_1
    @DailyDrivenBikes_1 Před rokem +1

    Your custom shop videos are awesome 👌

  • @Hijason74
    @Hijason74 Před rokem +1

    Great video. Keep the custom content coming!!!

    • @SMKWcom
      @SMKWcom  Před rokem

      TC loves making his EDC one of a kind 👍

  • @andrewrambeck5322
    @andrewrambeck5322 Před rokem +1

    Coolest scales I've seen

  • @AKAB_22
    @AKAB_22 Před rokem +1

    Doing this on my 20.5 ti next week!

    • @SMKWcom
      @SMKWcom  Před rokem

      Hope it turns out well!

  • @mikecurtis2585
    @mikecurtis2585 Před rokem +1

    Very nice looks great 👍

  • @ronaldmoore7698
    @ronaldmoore7698 Před rokem +1

    That's really cool

  • @skcamerican
    @skcamerican Před rokem +1

    Nice! That would be a cool finish on the ti Apta.

    • @SMKWcom
      @SMKWcom  Před rokem

      That would look awesome!

  • @carlholmes9858
    @carlholmes9858 Před 6 měsíci +1

    Is it really that easy?!?
    I can not, not do this now
    Thanks for posting

    • @SMKWcom
      @SMKWcom  Před 6 měsíci

      Let us know how it turns out!

  • @silverbeard_edc4546
    @silverbeard_edc4546 Před rokem +1

    PM3 is a great EDC. Nice job on the scales!

  • @Zaque-TV
    @Zaque-TV Před rokem +2

    Friendly observation: your intro music is 5x louder than the rest of the vid

    • @SMKWcom
      @SMKWcom  Před rokem

      Thanks for letting us know

  • @campuscolt65
    @campuscolt65 Před rokem +1

    Does that work on copper too ?

  • @Greg-zr4wm
    @Greg-zr4wm Před rokem +2

    Great video, my only issues as someone who has been burnt pretty good / bad in the past.
    I wouldn't suggest wearing those gloves when using a torch. If you had an accident they'd melt right into your skin.
    Definitely not a pleasant feeling having a burn site scrubbed clean.

    • @SMKWcom
      @SMKWcom  Před rokem +1

      Always take safety precautions and wear PPE to help prevent accidents from happing. Thanks for watching Greg 👍

  • @shaggy_e210
    @shaggy_e210 Před rokem +1

    Tempted to do this on mine. Damn near the same exact knife, I just have Flytanium scales.

    • @SMKWcom
      @SMKWcom  Před rokem +1

      Should work about the same then, let us know how they turn out 👍

  • @chrispage8087
    @chrispage8087 Před rokem +1

    Great tutorial I have a question though what kind of container should I use for the ferric chloride when quenching it and for storing it after

    • @SMKWcom
      @SMKWcom  Před rokem

      The Ferric Chloride comes in a plastic container but we use a glass jar like what we used in the video as an extra safety for the heat from the flames

    • @thundercell13
      @thundercell13 Před 4 měsíci

      Lots of people use mason jars to store theirs in so just throw a lid on it and store it till use it again. (Obviously the lid is usually metal) but as long as you don’t go shaking around all the time should be fine

  • @abgarza911
    @abgarza911 Před rokem +1

    Will pure acid works too?

    • @SMKWcom
      @SMKWcom  Před rokem

      We use ferric chloride acid so we can't speak to what works more. Always do research and use safety equipment

  • @FirstLast-qj6lh
    @FirstLast-qj6lh Před rokem +1

    What was the first thing you dipped it in after heating? Water and then rinse with water?

  • @vonster22
    @vonster22 Před rokem +1

    nice

  • @mike212916
    @mike212916 Před rokem +1

    you should have spoke more about technique. like how to get more of the electric look. Like more or less heat..how you dip it into the acid.. how long..

    • @SMKWcom
      @SMKWcom  Před rokem

      Thanks for watching and the suggestions as well

    • @ThisMightBeABadIdea
      @ThisMightBeABadIdea Před rokem

      They weren't doing a lightning anodization tho, he was doing a entropic. If you want an electric lightning style, you're watching the wrong video. Read the title or watch the whole thing next time

  • @jasonlong8625
    @jasonlong8625 Před rokem +1

    Looks great TC, did you use the Jantz ferric chloride etching solution listed on the SMKW website?

    • @SMKWcom
      @SMKWcom  Před rokem

      Yep! That is the one 👍

  • @MeskDaKrull
    @MeskDaKrull Před rokem +1

    Dude this looks absolutely stunning. Did i get you right that i could do this to a set of orange peel textured scales with similar results? How does it differ? Thanks

    • @SMKWcom
      @SMKWcom  Před rokem

      Obtenir un couteau avec du super acier signifie souvent qu'il est plus difficile à aiguiser mais que vous n'avez pas besoin de l'aiguiser aussi souvent

  • @jordanmyers0326
    @jordanmyers0326 Před rokem

    So how do you get rid of the acid afterwards

  • @mixgashaulass2988
    @mixgashaulass2988 Před 10 měsíci

    I have a stonewashed titanium knife, what results do you think I would get?

  • @dommorris8163
    @dommorris8163 Před 3 měsíci +1

    Is the ferric chloride diluted at all?

    • @dommorris8163
      @dommorris8163 Před 3 měsíci +1

      Nevermind I used 1 part FC mixed with 2 parts water and it worked perfectly. I had no idea it was this easy. Looks amazing

    • @SMKWcom
      @SMKWcom  Před 3 měsíci

      Nice! Keep playing with your mixtures and voltage to get something truly unique as well

  • @DudesIn101
    @DudesIn101 Před rokem +1

    Is it worth it,well HELL Yeah!!Totally makes the knife unique,oh my grandpa ask me one day,he said son how do you catch a rabbit,I well unique up on it and hit it with a 22....Beautiful knife,one day it will be up for auction on some well auction,great vid love the chann we'll see ya!

  • @Sharper_Than_Most
    @Sharper_Than_Most Před rokem +1

    Personally I like this style better then the “ lightening” ano!!

    • @SMKWcom
      @SMKWcom  Před rokem

      Could try mixing the two for lighting flames!

  • @isaiahbarnett9062
    @isaiahbarnett9062 Před rokem

    So with my birthday money I want to get the D2 od green minimalist. But they're out of stock, any idea when they will be back in?

  • @superrad1659
    @superrad1659 Před rokem +1

    How does the "lightning" pattern come through? Is that just what happens when it's quenched in the -water- oil? Is there a way to control the "entropic-ness" of the pattern/finish?

    • @litsci4690
      @litsci4690 Před rokem +1

      READ the screen. It's NOT water.

    • @superrad1659
      @superrad1659 Před rokem +1

      @@litsci4690 *oil, my mistake.

    • @SMKWcom
      @SMKWcom  Před rokem +1

      This pattern is after quenching in Ferric Chloride Acid and the main control is the heat how dark you get it when torching really sets up the pattern... I did not heat mine evenly because I wanted the variation, but with a more even heat you get a more consistent pattern.

  • @808DC2R
    @808DC2R Před rokem +1

    Awesome scales where did u buy that?

    • @SMKWcom
      @SMKWcom  Před rokem +1

      All the links are in the description but here is the one for the scales as well www.smkw.com/smkw-para-3-titanium-handle-scales

  • @5shotsr611
    @5shotsr611 Před rokem +1

    What kind of metal is them scales?. Looks koool 😎

    • @SMKWcom
      @SMKWcom  Před rokem +1

      www.smkw.com/smkw-para-3-tita...

  • @troublewells8777
    @troublewells8777 Před rokem +1

    Looks amazing!

    • @SMKWcom
      @SMKWcom  Před rokem

      TC did awesome! Thanks for watching TW

  • @joekasperek1086
    @joekasperek1086 Před rokem +1

    Nice TC did they give you any kind of discount because of Who You are?

    • @SMKWcom
      @SMKWcom  Před rokem +2

      We charge TC double for most things just out of principal

  • @ahealthylife3116
    @ahealthylife3116 Před rokem +1

    Bu metallerde olurmu

    • @SMKWcom
      @SMKWcom  Před rokem

      www.google.com/search?q=metals+that+can+be+anodized&oq=metals+that+can+be+anoized&aqs=chrome.1.69i57j0i13i512j0i390i650l2.10128j0j7&sourceid=chrome&ie=UTF-8

  • @TheFreak297
    @TheFreak297 Před rokem +1

    What do you dip the scale in after heating? Water to quench? Thanks

    • @litsci4690
      @litsci4690 Před rokem +1

      Water to get the ACID off!

    • @SMKWcom
      @SMKWcom  Před rokem

      It is a Ferric Chloride Acid used for etching.

    • @SMKWcom
      @SMKWcom  Před rokem

      Ferric Chloride Acid

    • @TheFreak297
      @TheFreak297 Před rokem

      @@SMKWcom thank u

  • @kniceslice780
    @kniceslice780 Před rokem

    Looks Smoky cool TC! Would this process work on a stainless handle?

    • @Zaque-TV
      @Zaque-TV Před rokem +1

      Not exactly. With steel it'll turn colors under heat but not as crazy. Also ferric chloride will etch up the finish so you wanna go straight to water once you see the color you want with the torch.

  • @stowfam
    @stowfam Před rokem

    What do you recommend to clean these and keep the finish bright and vibrant?

    • @SMKWcom
      @SMKWcom  Před rokem

      I would recommend something like case paste or flitz to periodically clean but they are relatively easy to just wipe down.

    • @jayrad017
      @jayrad017 Před rokem

      Windex

  • @mikemckenzy
    @mikemckenzy Před rokem

    How hot did you get the scale before quenching in the water? I haven’t had much luck with heat anodizing. I think I always get the titanium too hot.

    • @SMKWcom
      @SMKWcom  Před rokem

      I don't go by specific temperature, I just heat them until they start to change color and then the key is quenching them in Ferric Chloride Acid... that is what I quench them in, afterward I rinse them in water.

    • @sAssclown
      @sAssclown Před rokem

      When you get them too hot, does a lot of the color go away after quench?

    • @mikemckenzy
      @mikemckenzy Před rokem

      @@sAssclown yes. I never get the bright blues and purples. Always more muted. Like bronze and some dark blurple. It’s a neat finish but not what I’m trying to accomplish.

  • @zakariaott
    @zakariaott Před rokem +1

    You forgot the most important part...you gotta clean with acetone/alcohol before ano!

  • @slappynoname
    @slappynoname Před 4 měsíci +1

    I know you talked about safety in this video in regards to gloves and eye protection. You failed to mention thou that ferric fumes are highly carcinogenic to your lungs and can serious long lasting effects if it's not done in a well vented area, while also wearing a mask that is chem rated. I know the intent of this video was to show how easy it is to put a cool finish on some scales but not even mentioning that stuff seems like a big miss. Ferric is no joke and will mess you up.

    • @SMKWcom
      @SMKWcom  Před 4 měsíci

      You should always wear PPE and work in well ventilated areas. Take TC's advice, don't do as he does lol

  • @James-blond007
    @James-blond007 Před 9 měsíci

    I think u shudve emphasized the importance of safety especially dealing with ferric chloric acid!!

  • @kevinAuman1
    @kevinAuman1 Před rokem +1

    Yeah so on my birthday I get the spyderco PM2 in fat carbon uncoated M4 and when I opened the pkg the spydie box had a rubber band around it, so I opened that to find somebody's greasy fingerprints all over the blade and their arm-hairs!!! Wowwww was I disappointed, if I wanted you to test out my knife for me I'd ask also I kind of prefer the patina to be my own DNA so don't sell a knife that you have "USED" to display or to make videos as a "NEW-NEVER USED" knife because you have certainly "USED" it have you not?!?!? I've spent tens of thousands of dollars at SMKW and you've just lost a customer

    • @kevinAuman1
      @kevinAuman1 Před rokem +1

      There was also a big flat spot on thee edge apex where it must have been dropped, to a user im sure these things would not matter but I am a knife collector with intent of future resale but I certainly cannot sell this as an unused knife because that is not what it is at all and you should not have either!!!

    • @SMKWcom
      @SMKWcom  Před rokem

      I apologize for this we have a 30-day return policy if you will contact our customer service department at 800-327-5871 Monday through Friday from 9 am to 6 pm EST they will be happy to assist you.

  • @mitch511
    @mitch511 Před 6 měsíci

    Where do u get the acid? All I did is apply heat to get the blues and purples in a exhaust tip style fashion on a TI light and pen oh well haha

    • @michaell397
      @michaell397 Před 6 měsíci

      I ordered thru Amazon. 20 bucks for a quart. ;