Sir nice explanation sir Zara har cheez ki detail bta diya krien solutions kiss composition k bnany hain sir solution preparations bta dien or percentage b please
Sir make a video on how to do lacquer plating on iron and Copper jewellery by the process of copper synide where we skip the nickel part ! Thank you in advance..
Very nice information sir .... Because plating onto aluminium is very sensitive to these problems you said.
Sir nice explanation sir Zara har cheez ki detail bta diya krien solutions kiss composition k bnany hain sir solution preparations bta dien or percentage b please
Ok
Can you share a video for hard chrome coating plz
Acid copper ka anti tarnish ka nam kiya ha..??
Sir ak video nickel ke chemical ki banye kon kon s chemical use hote h
Sir make a video on how to do lacquer plating on iron and Copper jewellery by the process of copper synide where we skip the nickel part !
Thank you in advance..
Ok
Bright nickel ka Additive 220, spectra 977 or additive 22, brightner 33 ka farak kiye ha..??
सर ब्राइट टिन भी वीडियो बनाई है
Acid copper plating me choloride bar gaya to kiya kare..??
Pani ko dilute keren
Sir ph pepar ke bare me video banay
Sure
Bright nickel plating 220v current rectifier me plating hoga kya..??
Voltage DC chahiae 0-12 volt variable
Sir कृपया alkaline tin plating pr video bnayiye
Ji jaroor
Bright nickel plating ka pani tap water se banega kiya..??
Ji han
Sir nickel k 3 brightner ka kya name h
Brightner
Additive
Leveller
Sir brass murtiya ko bright shine ka 1 practical video banaye lacquering ke saath
Ji bilkul
Hame kaam chalu karna hai sir please help
Pls ek video dye gold lacquer ka bath kaise banta hai per banao
Ji ok
Bright nickel plating me growel ka spectra 977 acha ha ye brightner 33 acha ha..??
33
4 feet length tank 500liter pani me anode busket kitna dena ha..??
6 basket minimum
Electrolyte zincating me volt kitne dene hongy??
Zincating mein current nahin dena hei
It's dip process only 30 sec
Hi sir me pakistan si ho awr moji nickel me parblam aty hay mal jal jatahay ye karnt ka masla hoskta jay
Current problem and check boric acid concentration in chemical
Temperature should be 50 degree minimum
DM water processing, please
Ok
Bright nickel plating me dm water use karta ha..??
Ji dm water accha rehaga
Tap water se hoga..??
Ji bilkul
English please??
Sir nickel m kalapan aye toh kya kre
Sir plz reply dijiye
Sir bta dijiye
1 Brightner adhik dala hoga
2 current kem ho sakta hei
3 Pani mein copper ya zinc ka
Impurities ho sakta hei
Sir nickel plate kaha sea Lea kon c le
Inco
Hamare pas bhi mil jati hei
Sir aapko phone kiya whatsapp kiya tha sir aapne kuch bataya nahi
भाई सर का व्हाट्सएप नंबर सेंड करना
9837440016
Sir pls apna send krdo
9837440016
Awr ap jo nmbr hay whtsp ka mere whtsp pi nahai ata q
9410235861
Apna no bhejo
Sar ji apna Mobil no batado
9837440016
hello sir aap ka number chaheye
9837440016
Sir nickel k 3 brightner ka kya name h
Additive
Brightner
Leveller
Sir nickel sodium kis kam ata hai
Nickel sodium nam ka koi chemical nahin hota hei
Sodium hydroxide
Sodium hydroxide
Ye nickel ka chemical nahin