  • in this video i will show you how to make gold solution for silver plated
    #howtomakegoldsolution
    #jewelryplating
    #rosegoldplatedjewelry
    #platingsolution
  • Jak na to + styl

Komentáře • 389

  • @jadenephrite
    @jadenephrite Před 2 lety +72

    Thank you for your video. Regarding 0:40, the chemical formula for Potassium Cyanide is KCN. Caution must be used whenever handling cyanide, because cyanide could be fatally poisonous if it is ingested, inhaled or absorbed through bare skin. Regarding 2:25, combining 1 part nitric acid + 3 parts hydrochloric acid produces nitrohydrochloric acid, which is also known as Aqua Regia. Regarding 7:43 gold electroplating solution, if pure gold is used on the anode instead of stainless steel, then the gold electroplating solution will last much longer. This is because the gold cations in the electroplating solution will not become depleted since they will be replenished from the gold anode.

    • @expgame71
      @expgame71 Před 2 lety +7

      Is potassium cyanide mandatory for the proper functioning of the plating? Is it possible to replace it with another chemical element that is easier to find?

    • @jadenephrite
      @jadenephrite Před 2 lety +11

      ​@@expgame71 Thank your question. Gold electroplating can indeed be performed without the use of cyanide. Alternatives to the use of potassium cyanide is to use either sodium gold sulfite or to use potassium gold sulfite.

    • @expgame71
      @expgame71 Před 2 lety +3

      @@jadenephrite ok thank you for your reply. How to make sodium gold sulfite and potassium gold sulfite, is nitric acid needed?

    • @expgame71
      @expgame71 Před 2 lety +3

      @@jadenephrite yes but the problem with the solutions already made is that it is very expensive for very little gold, I would like to be able to make it myself

    • @aru_1396
      @aru_1396 Před rokem

      What is the toxicity percentage of potassium cyanide used and what is the grade of KCN

  • @vishalsambrekar
    @vishalsambrekar Před 2 lety +1

    Thank you so much.i am goldsmith .i am watching everywhere,asking everyone bu they dont tell me how to make gold plating solution.your video is best instructor to me. thanks

  • @HR_SAINI
    @HR_SAINI Před 2 lety +5

    You are teaching a masterpiece💗💗

  • @vishwanathsah8657
    @vishwanathsah8657 Před 2 lety +3

    No one explained like this well done bro

  • @phool289
    @phool289 Před 3 lety +2

    Very easy to understand thank you so much 💝

  • @vanjasemic8198
    @vanjasemic8198 Před 3 lety +3

    I cant believe!!!! Its wonderful!!! Congratulations

    • @AnifG
      @AnifG  Před 3 lety +1

      Thank you so much 😊🙏

  • @alexandrerodrigues3531

    Parabéns!
    Belo trabalho 🙏

  • @georgejosh1873
    @georgejosh1873 Před 3 lety

    Bang itu air merahnya kalo ga dicampur sama yang emas bisa buat dasaran sepuh ga? Biar merah dulu baru disepuh emas gitu?

  • @johnkaka1000
    @johnkaka1000 Před rokem

    Thank you so much. It’s a great help.

  • @manishkumarpatidar7000
    @manishkumarpatidar7000 Před 3 lety +3

    VERY USEFUL THANKS.A LOT.

  • @dongbotang
    @dongbotang Před 2 lety +1

    Great video! Many thanks from Australia.

    • @AnifG
      @AnifG  Před 2 lety

      Thank you so much.. greetings 🇮🇩

  • @hermanrany3325
    @hermanrany3325 Před 2 lety +1

    Assalamualaikum bang, mau nanya.
    Bagusan mana sepuh merah dulu atau sepuh putih perak dulu sebelum proses sepuh emas?🙏

  • @Fashion.jpeg_
    @Fashion.jpeg_ Před rokem

    Can this solution be used on 3d printed items? Do I need to spray anything on the 3d printed item first if so?

  • @alejandrogracia4448
    @alejandrogracia4448 Před 3 lety +11

    This is priceless, thank you so much! 🙏

    • @AnifG
      @AnifG  Před 3 lety +1

      Thank you so much sir😊🙏

  • @leleaquino1312
    @leleaquino1312 Před rokem +4

    Thank you for your video. In Brazil I didn't find any video talking about the chemical part of gold solutions
    How many times can this solution be used? Can I use up to how many grams of jewels without losing the gold?

  • @pbjsilverstudio4882
    @pbjsilverstudio4882 Před 3 lety +2

    Saved this video!! Thanks!

    • @AnifG
      @AnifG  Před 3 lety +1

      Yes ma'am.. thank you very much 😊🙏

  • @solmaz.khorashadi
    @solmaz.khorashadi Před rokem

    Thank you for your helpful video. I have a QUESTION, is it possible to make the rosegold solution into rosegold powder?

  • @sirbinyamin7636
    @sirbinyamin7636 Před 2 lety +3

    Hello, Can you let us know where did you get all the chemicals you are using? because in my country I try over and over but it is simply impossible to find them or they want to sell them by huge quantity... thanks 😀

  • @mohideenanver3700
    @mohideenanver3700 Před 2 lety

    Thank you so much for sharing plating process

  • @MetalGearIV
    @MetalGearIV Před 2 lety

    wow you are a gift for humankind

  • @ricojuliusretardo7510

    Thank you for sharing your Idea ,I really appreciate in you😁

  • @avivhanale3174
    @avivhanale3174 Před 3 lety +4

    Hello sir can you tell me how to make brighter for this solution

  • @sliceofbrain_
    @sliceofbrain_ Před 2 lety

    Thankx for sharing your knowledge. May I know what is name of the electric machine you are using. And where can I buy it?

  • @kndblade
    @kndblade Před 2 lety +1

    Definitivamente eternamente agradecido, muchísimas gracias saludos

  • @Gazanferylmaz
    @Gazanferylmaz Před 2 lety +2

    Will, we encountered a problem such as gold sinking over time?

  • @satheeshkumar-un6rl
    @satheeshkumar-un6rl Před 2 lety

    Superb demonstration

  • @cabulingue
    @cabulingue Před 3 lety +2

    Terima kasih banyak Pak Anif G, Saya doakan bapak selalu sehat, banyak rejeki n berumur panjang teruslah bikin konten yang bermafaat.
    pak cara buat yg rose gold itu pakai campuran CU tadi ya,
    salam

    • @AnifG
      @AnifG  Před 3 lety

      Amin.. terimakasih banyak om..🙏..iya betul om untuk rosegold saya pakai Cuso4/terusi.. atau bisa juga pakai yang sudah menjadi larutan

  • @arifinpanegoro6882
    @arifinpanegoro6882 Před 2 lety

    Pakai berapa volt mas? Apakah voltase juga pengaruh ke kekuatannya?

  • @machruskenzo7346
    @machruskenzo7346 Před 2 lety

    Thanks you very much 👍,,, good luck bro 👍

  • @marinnicolae4215
    @marinnicolae4215 Před 2 lety +23

    A nickel coating is required beforehand because the silver or copper atoms migrate to the outside and discolor the gold

    • @2ndPortal
      @2ndPortal Před rokem +4

      Why, his attempt looked great. Are saying with time?

    • @travismiller5548
      @travismiller5548 Před 11 měsíci +1

      Why nickel comes before chrome as well.

    • @lenny108
      @lenny108 Před 9 měsíci +1

      Some say the best is to have chrome. On Amazon they sell gold electrolyte that is supposedly abrasion resistant. How is this achieved? Abrasion-resistant gold plating?

    • @RahulPatel-kk1ci
      @RahulPatel-kk1ci Před 8 měsíci +2

      nickel or chrome coating is good but not good for the skin so avoid to do

    • @newmonengineering
      @newmonengineering Před 7 měsíci +4

      ​@RahulPatel-kk1ci if you don't use nickel, the silver will tarnish under it and slowly discolor the gold. Most gold plated things are a very thin coating of gold. You can however go thicker to say 2.5 microns and it's a much better protection but also significantly more costly to do. Often they will use rhodium as a base layer over silver if they don't use nickel

  • @nyomanngetis6329
    @nyomanngetis6329 Před rokem

    Maaf boss, untuk sepuh rose gold apakah bisa buat ketebalan tertentu?

  • @techsvayrieng3280
    @techsvayrieng3280 Před rokem

    Good brother,thank you.
    Have Other solution for make it bright or not?

  • @jacquesomersavard7257
    @jacquesomersavard7257 Před 2 lety

    I have lot of electronic gold part is it possible to use it in this process

  • @pratishshrestha9623
    @pratishshrestha9623 Před 2 lety +1

    How long does it last??

  • @chrissmith841
    @chrissmith841 Před rokem

    Does it work out much cheaper making it yourself than buying ready made? thank you

  • @jacquesomersavard7257
    @jacquesomersavard7257 Před 2 lety

    is it possible to make this whit stain glass copper frame or lead frame

  • @rayaraya6720
    @rayaraya6720 Před 11 měsíci

    Potasium pakai potas apa ya mas agar air sepuhan tidak cepat berubah keruh

  • @bernardkorley6946
    @bernardkorley6946 Před rokem

    So how long will such a playing last normally before you would have to plate it again

  • @nilupul84
    @nilupul84 Před 2 lety +1

    Hi Dear, I try it gold plating is really good. but something wrong in my solution. some brown dust making on SS Anode.
    can you tell me. HCL,HNO3,KCN & Water quantity for 250mg 24k Gold .
    Thanks

  • @amyelaja3614
    @amyelaja3614 Před 3 lety +1

    Bang numpang nnya juga ni sama ahlinya..
    Kalao untuk pemerah harus pakai potassium cyanide..
    ?? Yang berapa persen bang..??
    Makasi infonya..

  • @user-yk9ee4jk1u
    @user-yk9ee4jk1u Před rokem

    Thank so mach for this interesting video but i am just wondering of using potassium or potassium cyanide

  • @Sjchrome24
    @Sjchrome24 Před 2 lety

    Please provide a tutorial for the yellow silver encoding of white without the use of rhodium

  • @detectormaniaindonesia8131

    Any working PH for this plating? Thanks

  • @ArshadAli-ny3dr
    @ArshadAli-ny3dr Před 2 lety +1

    Which metal is the ring you used? And can I do this color on aluminum

    • @AnifG
      @AnifG  Před 2 lety

      It's silver...you can't use this solution for alumunium

  • @randyreyes8689
    @randyreyes8689 Před rokem

    Thank you for your video, thank you very much

  • @Avci__
    @Avci__ Před 2 lety

    Can you explain in the same solution how to paint gold in a yellow color and a color similar to copper?

  • @mochamadvidal4186
    @mochamadvidal4186 Před rokem

    Mantap boss.
    Kalau boleh tahu, tinggalnya dimana..?

  • @harsharohan88
    @harsharohan88 Před 2 lety

    Hi sir
    Use distilled water or normali pio water . please help me thanks

  • @byanarga2387
    @byanarga2387 Před 3 lety +1

    Thank you so much

  • @rajasasitepu9531
    @rajasasitepu9531 Před 6 měsíci

    Bang Anif, sdh like n subscribe. Saya sdh tonton video part 1 dan 2 ini. Makasih. Tapi nanya ini, apakah semua obat/zat kimia itu bisa dibeli bebas di toko kimia? Itu aliran listrik saat ngerendam cincin, pake brp volt itu bang. Thanks.

  • @helloitsanxiety6234
    @helloitsanxiety6234 Před rokem

    hi! what about silver 925 plated things? i have a necklace that is indian silver, since it's old and i cleaned it very aggressively last time, a brassy color came out 🥲so now i have a necklace that is a spotted coloration 😭i was thinking of coating it in silver 925 but i don't know how...i'd like to do it myself cause i'm poor but my dad used to make handmade jewelry so i have some equipment, also i like to learn new things. could you hand me some tips? thank you so so much
    (also i'm form italy so forgive my poor english pls)

  • @essamliana8232
    @essamliana8232 Před rokem

    Untuk elektroplating perak pakai apa y?

  • @InfinityJewellery06
    @InfinityJewellery06 Před rokem

    Can 14k gold be played in this solution

  • @lokeshman1710
    @lokeshman1710 Před 2 lety

    is it the same process if I need do a bath electro plating in copper statues?

    • @sirbinyamin7636
      @sirbinyamin7636 Před 2 lety +1

      The best to plate copper is first nickel plated and after gold plated

  • @algeriano5424
    @algeriano5424 Před rokem +1

    please, if we want the color of green gold and blue for example, what sulphate is needed to achieve it, and a thousand thanks for this important video, I await your answer

  • @MrMo7emad
    @MrMo7emad Před 3 lety +2

    İ don't know how to thank you
    İt's very useful video

    • @AnifG
      @AnifG  Před 3 lety

      You're welcome, sir 😊🙏

  • @nurettingencturk1124
    @nurettingencturk1124 Před rokem

    are we going to neutralize three parts of hydrochloric acid and one part of nitric acid ? thanks.

  • @sofiahearts4625
    @sofiahearts4625 Před 3 lety +1

    Best video thanks..........👍

    • @AnifG
      @AnifG  Před 3 lety

      Thank you so much 😊🙏

  • @hyperhidrosissupport9186
    @hyperhidrosissupport9186 Před 10 měsíci

    can i use potassium ferrocyanide instead of cyanide ?

  • @ishqesahil8864
    @ishqesahil8864 Před 2 lety +1

    Anif I want to gold plate surgical instruments. Can you please tell me what proportions of ingredients are used in yellow gold plating and what is the lifetime of this plating?

  • @plumbum1153
    @plumbum1153 Před 8 měsíci

    Excellent !!!!

  • @karangandhi5216
    @karangandhi5216 Před 3 lety

    Hello sir,
    Plz illustrate How to make redish polish for gold chain

  • @gonzalovaldez8204
    @gonzalovaldez8204 Před 3 lety +7

    Hello, it is an interesting process, when you brown a ring, the liquid that remains is discarded no longer works, how resistant is the gold, how do I make it last longer, I have seen you do other processes of black. as it does. can you teach me. saludos desde Colombia

    • @akhmadfazar7004
      @akhmadfazar7004 Před 2 lety

      Kalo buat 100 potong emas brp takaran emas untuk di larutkan?dan talaran hno3 sama hcl nya jadi brp gan?🙏

    • @muchniksolo4980
      @muchniksolo4980 Před 2 lety

      @@akhmadfazar7004 biasanya dijitung dr berat mas yg akan di plaiting,aku sendiri jg buat dgn cara itu utk bahan emas 0,25grm dpt menghasilkan kurang lebih 1kg,semoga membantu🙏

  • @dusanstanic1462
    @dusanstanic1462 Před 3 lety +4

    Can stainless steel be plated and what is the procedure (preparation etc)? And how durable is this plating? Thank you

  • @Avci__
    @Avci__ Před 2 lety

    Can I not add cuso4?

  • @MegaUsman42
    @MegaUsman42 Před 3 lety +2

    Can you please tell, how much time per mg is required. Or how much time is sufficient to electroplate jewellery

  • @tonykarlsson8589
    @tonykarlsson8589 Před 11 měsíci

    Good job 😊

  • @umargul5644
    @umargul5644 Před 2 lety

    Great 👍 thanks

  • @aitamerabdrrahim7823
    @aitamerabdrrahim7823 Před rokem

    Please how do I get the 18k paint solution what is the composition

  • @BALITEKNIK070809
    @BALITEKNIK070809 Před 3 lety +1

    Wow mantap tutorialnya, sukses buat channelnya

    • @AnifG
      @AnifG  Před 3 lety

      Terimakasih om.. sukses juga buat anda 😊🙏

  • @hargrim6892
    @hargrim6892 Před 3 lety +1

    @Anif G, HCl sama HNO3 itu pakai yang berapa persen ya? kalau di pasaran saya lihat ada yg 32% sama 65%

    • @AnifG
      @AnifG  Před 3 lety

      Semakin tinggi kadar kemurnian ,semakin bagus bang,,

  • @ccezar84
    @ccezar84 Před 3 lety +2

    Hello Anif. How thick can you plate with this solution without getting dull? Can you achive 2 microns of bright gold plating?
    This solution plate on non-ferous only? How good is the adhesion?

    • @AnifG
      @AnifG  Před 3 lety +1

      Thanks for watching, I don't understand the answer to your question, but as far as I am it is the cheapest way to get the gold solution, and I always use it

    • @isawalter3465
      @isawalter3465 Před 3 lety

      can you please explain that ? I just know this channel and never saw, he says something about dumbness beyond 2 microns ... sorry german but the guy is super experienced ..
      czcams.com/users/RolandBetzmannRealGoldvideos

    • @isawalter3465
      @isawalter3465 Před 3 lety +1

      @@AnifG Hi dear Anif, amazing! I am following this channel. He recommends 3micron for average use up to way more depening on purpose.
      Is your solution limited regarding micron thickness? thank you! Are you on Facebook for PN? thank you! :-)

  • @user-mp6vf3xg7v
    @user-mp6vf3xg7v Před rokem

    Hello,
    I have prepare the plating solution as per your instructions, but the colour of the plating is black in colour. Please clarify. We want to know the exact amount of HCL and HNO3. Thank you.

  • @karangandhi5216
    @karangandhi5216 Před 3 lety +5

    Hello sir,
    Thank you for ur vedio
    If we dissolve 1 gm how much gms we can polish for 24k

  • @hobiaja7666
    @hobiaja7666 Před 2 lety +1

    Ada yg jual air sepuhan jadi tinggal pake nggk mas yg kayak itu.....?
    Terimakasih

    • @AnifG
      @AnifG  Před 2 lety

      Di toped ada bang

  • @brdmec134
    @brdmec134 Před 3 lety +3

    Absolutamente divino! Parabéns

    • @AnifG
      @AnifG  Před 3 lety

      Thanks for watching

  • @wawanrustiawan1201
    @wawanrustiawan1201 Před 3 lety +1

    Pak hanif. Kalau mau ngelapis emas di cincin berbahan stainless, ga bisa langsung kaya di video ya? Apa ada tambahan campuran khusus?

    • @AnifG
      @AnifG  Před 3 lety

      Kalo untuk stainless gak bisa bang..ini cuma bisa untuk melapisi tembaga, alpaka, perak sama emas

  • @masoodsheikh4600
    @masoodsheikh4600 Před 3 lety

    After Gold Plating can we pour the used Solution back into the Bottle or waste it
    If pour back into bottle then how long can we use it?

    • @byanarga2387
      @byanarga2387 Před 2 lety +3

      used solution usually saved in another bottle. 1L solution can be used for about 1kg jewelry

  • @sachinlohar1106
    @sachinlohar1106 Před 2 lety +1

    Sir isme kitna kam niklta hai

  • @randimadanthanarayana3839

    Thank u sir. Its really helpful for me. Sir, i did this same as your video. And i plated. Rings, pendents. after plating its really nice and success. But it is not possible for chains. Chains are got black and very ugly colour. Can plz advice me sir.

  • @billmusik9794
    @billmusik9794 Před 8 měsíci

    can you use sodium Cynide ?

  • @agusmulyana9164
    @agusmulyana9164 Před 2 lety

    Bang lama kelamaan kok jadi agak hitam penyebabnya apa biasanya? Ini buat berapa gram perak

  • @harishrajamani4922
    @harishrajamani4922 Před 3 lety +3

    How to make cyanide free gold polishing Solution?

  • @dannysoni3518
    @dannysoni3518 Před 2 měsíci

    Does we need surface activator for gold plating on silver ... if yes tjen how can i make that

  • @thetruth1989
    @thetruth1989 Před rokem

    Sir how do you get the 24k gold color not yellow gold color

  • @billmusik9794
    @billmusik9794 Před 7 měsíci

    Is that just plane potassuim?

  • @takishidz7961
    @takishidz7961 Před měsícem

    Does it need a precise voltage amont to use and does it have any impacte on the final result

  • @gamelife7139
    @gamelife7139 Před 10 měsíci

    Hi Bro, thank you for video
    have a Quistion
    How make lemon yellow color for gold plating? (mean lighter yellow than 24k like lemon)
    thank you❤

  • @sirbinyamin7636
    @sirbinyamin7636 Před 2 lety +5

    Hello, does anyone know where to buy those products? A internet site or any other place would be really helpful. Thank you very much

  • @rstezza
    @rstezza Před 2 lety

    Can this be put into a air brush and sprayed on??
    How is 24k gold sprayed in like a water solution??

    • @goognamgoognw6637
      @goognamgoognw6637 Před rokem

      It's not. The only other way is with a brush, and that won't be as good as electrolytes.

  • @PCRcontents
    @PCRcontents Před 3 lety +1

    what M of HCl and NO3

  • @bling6646
    @bling6646 Před 2 lety +1

    Hey Anif,
    Thank you for this rare video. How can I make a 14 karat gold solution?

    • @joonaskekoni2867
      @joonaskekoni2867 Před 2 měsíci

      I would assume mixture of zink cloride snd copper suphate. I however fail so see why anyone wanted that.

  • @gplusgplus2286
    @gplusgplus2286 Před 2 lety

    How to gold plate with a gold sovereign as source of gold?

  • @franknieto2760
    @franknieto2760 Před 3 lety +3

    Potassium cyanide is very deadly. Where can you get it? Other than gloves and good ventilation, what precautions should one take?

    • @AnifG
      @AnifG  Před 3 lety +1

      yes it is very poisonous, I think a lot of materials for the jewelry production process are toxic, the important thing is to always maintain work safety with the right procedures

    • @armazrivera2302
      @armazrivera2302 Před 3 lety

      There is an internet page where you can find potassium cyanide

  • @padmanavajethy721
    @padmanavajethy721 Před 3 lety +1

    Good work. How to harden 24 carat gold. Any other metal could be used?

    • @AnifG
      @AnifG  Před 3 lety +2

      Thank you so much..😊🙏 For 24k gold solution it can be used to coat various jewelry made of gold, silver and copper

    • @padmanavajethy721
      @padmanavajethy721 Před 3 lety +1

      @@AnifG I am a goldsmith . I need to add some hard alloy with gold so that the gold coating becomes hard and the jewellery colour will last longer. Could any hard metal could be added to the solution?

    • @AnifG
      @AnifG  Před 3 lety +3

      For the addition of other metals besides gold, of course you can't sir, this method is only for 99% pure gold which is dissolved, the environment mixed with other metals such as alloys will certainly damage the solution, but if you want to make the coating more durable you can use a nickel solution whose video I will for coming 🙏

  • @shandyengraver
    @shandyengraver Před 3 lety +1

    Mas klo bikin sipuh 2 warna gimana caranya ?

    • @AnifG
      @AnifG  Před 3 lety

      Di video sy ada bang yang proses Kombinasi 2 warna

  • @GILBERTOMARTINEZSAUCEDO
    @GILBERTOMARTINEZSAUCEDO Před 10 měsíci +2

    Hi! my stainless steel plate started to corrode during the plating process, and contaminated the solution (green/orange) sediment do you know why this is ?

  • @famtovar5385
    @famtovar5385 Před 9 měsíci

    So can you reuse the gold solution after one time? If so how many times can i reuse it…. And should i remix with the rest of the solution (unused solution) ?

  • @donnieuhc402
    @donnieuhc402 Před 2 lety

    How do I get that ring bro

  • @EnriqueGuerreroO
    @EnriqueGuerreroO Před 3 lety +2

    If I want to 18K gold electroplate a carbon knife (opinel), can I use as anode a piece of 18k jewelry, and, as I don't have a gold solution, can I use simple sodium bicarbonate as my electrolite?

    • @AnifG
      @AnifG  Před 3 lety

      I don't understand about that, maybe someday I'll try to experiment about it

    • @AbdulKareem-lq3tr
      @AbdulKareem-lq3tr Před 2 lety

      Assalamu alaikum Haneef jee how to make cheepest gold solutions would yu pls reply