Casting Defects | Dental Materials | Super Simple
Vložit
- čas přidán 24. 08. 2024
- This video on Casting defects from Dental Materials includes defects like Porosity, Incomplete casting, distortion, and surface roughness. The casting defect topic is a very important topic for dental students and exam like MDS entrance NEET Exam, NBDE. The questions are generally on localized shrinkage porosity, Suckback porosity, Backpressure porosity. The video explains these things in a simplified way with diagrams too. Easy dentistry at Aspire32 helps grasp such topics of Dentistry in the simplest possible way for dental students and dentists. Casting defect in dentistry is a difficult topic.
This video of Aspire 32 is made by Dr. Suresh Shenvi who has cleared various exams like ADAT, NBDE from the USA, DHA from Dubai, and various Indian Entrance exams like PGI, KCET, NEET. I am MDS in Conservative Dentistry and Endodontics by profession. I am also an author of dental books on the entrance exam and I am also currently a faculty at KLE University and a receiver or best teacher award.
Click The Following Link To Subscribe To My Channel Aspire 32
www.youtube.co...
Link for Complete Playlist on Cast Restorations
• Inlay and Onlay - Cast...
Link for Complete Playlist on Fundamentals of Cavity Preparation.
• Fundamentals of Tooth ...
Link for Complete Playlist on Dental Composite
• Dental Composite
Link for Complete Playlist on Glass Ionomer Cement and its types.
• Glass Ionomer Cement (...
Link for Complete Playlist on Pulp and Periapical Diseases
• Pulp and Periapical Di...
Link for Complete Playlist on Pulp Protection ( Direct and Indirect Pulp capping)
• Pulp Protection - Varn...
Link for Complete Playlist various Dental Product reviews
• Review of Endodontics ...
#aspire32, #sureshshenvi,
Thank you so much sir , with clear concept help me a lot helping a lot in solving Mcqs in neet
Glad to hear that. I am happy the channel is meeting its purpose :)
I've never would've understand this topic if i did'nt see this.
You explained it so well! Thank you so much sir
Thank you for the kind words :).. That really made my day :)
Majestically put,
Full of wisdom and intellect.
Love and Respect from Kashmir.
Thank you so much dear :):)
Sir you explain soo well that everything seems so easy
A heartfelt thanks to you 😊
Thank you. I just explain the same thing which is there in textbook :)
Do Check the new video just released today.
Rotary Cutting instruments covers type of Handpieces, Speed, Types of burs, the various angle like Rake Clearance angle, Edge angle in a Super Simple Way !
czcams.com/video/Nqq9WkU1Xx8/video.html
Awsome
.videos....keep.uploading🙏🙏🙏👍👍👍👍👍👍👍👍👍👍👍
Sure. There are many useful videos. Do check them :) .. Hope you will Subscribe :)
Much needed topic. Wonderfully explained sir. ,👍👍
Thank you Pankhuri :)
Nicely explained..thnks😄
So glad..do check other videos
Thank you sir..Your videos going to help a lot ..
Welcome Vinod. Do share it with others :)
Tq so much sir it helped me a lot.
You are most welcome
I had read it like so many times but i dint get it, now i listened to this n went to pulse to solve MCQ, i could ans then all , thank you so much sir, no words 👏👏
Absolutely. Things do not have to be so complicated isn't it ?. I am glad you found it useful
Thank you so much for this awesome series of videos on Cast restorations.. Wish I understood cast restorations so clearly during the college.. Thank you once again and God bless you!!!
So happy to hear that you finally understood the topic better. Do check this video on prepration for cast Restoration. czcams.com/video/DqMaCXL7qpI/video.html
I was struggling with this topic... Finally got my concept cleared.. Thank you so much sir😊
This is what makes me super happy. Knowing its helping students understand better :) do subscribe to the channel
Here is are few more videos related to cast Restoration
czcams.com/play/PLdPsg6P-6VlcG-msLe6BvhIz9p3QYx4VY.html
Neatly explained sir.... upload more like this ....
Thank you Dr Ajay :)
You have a skill for teaching.
so happy to hear :)
Sir .....u and ur lectures are best....
Thanks for the appreciation
Thanku soo much sir..You explained every point to the deapth
Most welcome :):)
Best video 💯🙏🏽🙏🏽
Thank you sir.
So happy to hear that :)
Thankyou sir for making DM that much easier for us 💃😃
Most welcome. Do check the other dental Material videos here. Also do check operative videos on the channel
czcams.com/play/PLdPsg6P-6VldkI_N1LglBPGc114Ksq9Ir.html
Sir you mentioned that localized shrinkage porosity occurs internally and to visualize that , we need to cut through the casting..... Can you please explain this?. Rest everything was crystal clear... Thank you so much
It means that it happens internally. You dont see it usually
Sir please make a video on investment materials 🙏
I will definitely try :)
Helping a lot , thanks for guidance 🙏
Glad to hear that :). I hope you will check the other videos. Do check the dental Ceramics video if you always found that difficult too :)
This was really helpful, thankyou!!!
Most welcome. Do visit the playlist sections. I have made many more Simplified
How to decide which investment material to use for which wax which properties should be similar
It depends on the metal alloy one will be using for casting
🙏🙏🙏
Thank you. Pls do check
czcams.com/play/PLdPsg6P-6VlcG-msLe6BvhIz9p3QYx4VY.html
Sir can you please explain about class 2 modifications of cavity preparation
Yes, The topic is in my list.. Will make it .. Hope you checked my earlier video on class 2 Link czcams.com/video/_85BAZA6dxo/video.html
Simply amazing!!
Thank you. Hope you will check the other videos too :)
❤❤
Thank you :)
Excellent
Thank you :):)
Sir, please reply
When the metal shrinks on solidification, the shrinkage is towards which direction? How exactly the investment material expansion compensates for it ? Is the shrinkage towards outside? As shown at 2.45
I did mention about it in the video
Sir investment Powder what's how stor purchase
Super sir☺️
Thanks :)
Can u explain distortion (due to investment material) ...unable to understand please?
You mean when mould expand...can pattern also explain which leads to porosities ?
Yes. It pulls the pattern with it