Part 1 - Scientific Troubleshooting - Solutions for Common Injection Molding Defects
Vložit
- čas přidán 17. 02. 2009
- Join Andy Routsis, founder and president of A. Routsis Associates, as he presents a scientific troubleshooting framework for five of the most common injection molding defects.
By viewing this video presentation, you will gain an understanding of how to effectively document the injection molding process and determine what changes occurred to cause the defect. Andy's approach to troubleshooting is aimed at the cause, not the symptom, giving the attendee a solid understanding of what to do and most importantly, WHY to do it.
DOE's mean nothing if the clamp is off balance. Sometimes it is the press. Stable processes for years, Clamping motor took a crap. Replaced it and found 1 of the tie bars snapped after. There was no signs of wear. Sometimes it could be the things we dont check.
heat automatically increase , (zone2) how many defects in this problem ? Please answer to me
when you have to do 4 to 5 mold changes and start them up by yourself in an 8 hour time frame you do not have the time to do all of that.
My teacher need ur help
reason why the automatic door not close
You got to press cycle button then the door button then it shuts then press the circle button to complete the shot. Press the hand button once the shot has completed then press the door button then the door will open.
@@ashleybishton742 hello how I can calculate the shots for injection mold 4 cavities.... mold weight 25 grams and the machine is 180 ton
5 molds per day for one person ? Srsly ?
Unchallenged plckejankre
you guys dont know how to use DOE RSM here. study of parameter and response interactions should be clearly mapped using RSM. not just by experience and technical know how. you never mentioned DOE. or you tried DOE but unsuccessful.
Would you please explain more for using DOE RSM in injection molding?